Fingerprint
Dive into the research topics of 'Inertia welding nickel-based superalloy: Part II. Residual stress characterization'. Together they form a unique fingerprint.- Sort by
- Weight
- Alphabetically
Michael Preuss, J. W L Pang, P. J. Withers, G. J. Baxter