Inertia Welding Nickel-based Superalloy. Part II: Residual Stress Development

Michael Preuss, JWL Pang, PJ Withers, GJ Baxter

    Research output: Contribution to journalArticlepeer-review

    Original languageEnglish
    Pages (from-to)3227-34
    Number of pages3192
    JournalMetal. & Mater. Trans
    Volume33A
    Publication statusPublished - 2002