Intergranular Stress Corrosion Crack Propagation in Sensitised Austenitic Stainless Steel (Microstructure Modelling and Experimental Observation)
TJ Marrow, L Babout, AP Jivkov, P Wood, D Engelberg, N Stevens, Philip Withers, RC Newman
Research output: Chapter in Book/Report/Conference proceeding › Chapter