Projects per year
Abstract
Relatively low levels of inter-pass deformation have been found to be very effective in refining the coarse columnar grain structures normally seen in Ti-6Al-4V components, built using wire-fed high-deposition-rate additive manufacturing processes. The most important process parameters that control the level of β recrystallization – the final grain size and micro-texture – were systematically investigated by simulating the deformation and high heating rate conditions in controlled samples, to develop the process knowledge required to optimise inter-pass deformation and obtain predictable grain sizes. Overall, it was found that the level of β-grain refinement achieved by inter-pass deformation was surprisingly insensitive to the ranges of deformation temperatures, deformation speeds, and changes to the as-deposited α + β microstructure, expected within the WAAM process window, provided a minimum plastic strain of only 14% was achieved in each added layer. Conversely, the final component grain size was shown to be strongly affected by rapid grain growth on re-heating above the β transus. The texture results obtained were consistent with previous work which suggested that, with fine AM transformation microstructures, new β-grain orientations may be produced during the α → β transformation from the development of twinning faults, induced by the prior deformation and rapid heating. In contrast, greatly increasing the starting α lamellar spacing – to be more similar to that found in a wrought material – greatly reduced the level of recrystallization and also appeared to change the recrystallization mechanism to favour new β orientations produced largely by local lattice rotation.
Original language | English |
---|---|
Pages (from-to) | 110298 |
Journal | Materials Characterization |
Volume | 163 |
Early online date | 28 Mar 2020 |
DOIs | |
Publication status | Published - 1 May 2020 |
Fingerprint
Dive into the research topics of 'The effect of processing parameters on rapid-heating β recrystallization in inter-pass deformed Ti-6Al-4V wire-arc additive manufacturing'. Together they form a unique fingerprint.Projects
- 2 Finished
-
[NEWAM] New Wire-Additive Manufacturing
Prangnell, P. (PI), Pickering, E. (CoI), Robson, J. (CoI) & Shanthraj, P. (CoI)
25/06/18 → 24/06/24
Project: Research
-
LightForm: Embedding Materials Engineering in Manufacturing with Light Alloys
Prangnell, P. (PI), Curioni, M. (CoI), Haigh, S. (CoI), Quinta Da Fonseca, J. (CoI), Robson, J. (CoI), Shanthraj, P. (CoI) & Zhou, X. (CoI)
1/10/17 → 18/10/23
Project: Research