@article{b5696eea63194cc6b69e9371d3894e37,
title = "The sensitivity of Ni-based superalloy to hole making operations: Influence of process parameters on subsurface damage and residual stress",
keywords = "Bi-axial residual stresses, Drilling, Ni-based superalloy, Plunge milling, Workpiece surface integrity",
author = "J Kwong and {A Axinte}, D and PJ Withers",
year = "2009",
doi = "10.1016/j.jmatprotec.2008.09.014",
language = "English",
volume = "209",
pages = "3968--3977",
journal = "Journal of Materials Processing Technology",
issn = "0924-0136",
publisher = "Elsevier BV",
number = "8",
}